Resinex, Member of the Ravago Group
Saturday, October 19, 2019
Braskem PE TS7003
Units 
Braskem - Low Density Polyethylene
ActionLegend (Open)
E-Mail a Datasheet Print this Page  

General Information
Product Description
TS7003 is a low density polyethylene (LDPE) with high molecular weight that offers high mechanical strength and toughness even at low temperatures. Additionally, this product is easily processed .The product was developed to meet the requirements for automatic packaging. The additive package provides low coefficient of friction ­ COF, allowing high productivity on the packaging lines. This product is identified as PE 115 according to ASTM D-4976-04a standard specification.

Additives:
Antiblocking
Slip agent

Application:
Films for automatic packaging of liquids such as, milk, yogurt, juices, etc.
Packaging for frozen food: meat, chicken, seafood, fries, etc.
Blow molding flexible packaging.

Process:
Blown Film Extrusion
General  
Material Status 
  • Commercial: Active
Availability 
  • Europe
  • Latin America
 
Additive 
  • Antiblock
  • Slip
 
Features 
  • Antiblocking
  • Good Processability
  • Good Toughness
  • High Molecular Weight
  • High Tensile Strength
  • Low Temperature Toughness
  • Slip
Uses 
  • Blown Film
  • Film
  • Food Packaging
  • Packaging
 
Agency Ratings 
  • ASTM D4976-PE115
Processing Method 
  • Blow Molding
  • Blown Film
 
ASTM & ISO Properties 1
Physical
Nominal Value
Unit
Test Method
Density / Specific Gravity
0.922
g/cm³
ASTM D792
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg)
0.27
g/10 min
ASTM D1238
Films
Nominal Value
Unit
Test Method
Secant Modulus - 2% Secant, MD (70 µm, Blown Film)
140
MPa
ASTM D882
Secant Modulus - 2% Secant, TD (70 µm, Blown Film)
150
MPa
ASTM D882
Tensile Strength - MD (Break, 70 µm, Blown Film)
20.0
MPa
ASTM D882
Tensile Strength - TD (Break, 70 µm, Blown Film)
20.0
MPa
ASTM D882
Tensile Elongation - MD (Break, 70 µm, Blown Film)
380
%
ASTM D882
Tensile Elongation - TD (Break, 70 µm, Blown Film)
910
%
ASTM D882
Dart Drop Impact (70 µm, Blown Film)
230
g
ASTM D1709
Elmendorf Tear Strength - MD (70 µm, Blown Film)
300
g
ASTM D1922
Elmendorf Tear Strength - TD (70 µm, Blown Film)
220
g
ASTM D1922
Optical
Nominal Value
Unit
Test Method
Gloss
    ASTM D2457
45°, 70.0 µm, Blown Film
41
 
 
60°, 70.0 µm, Blown Film
54
 
 
Haze (70.0 µm, Blown Film)
20.0
%
ASTM D1003
Notes
1Typical properties: these are not to be construed as specifications.
 
Customer is responsible for determining whether products and the information in this document are appropriate for Customer’s use and for ensuring that Customer’s workplace and disposal practices are in compliance with applicable laws and other governmental enactments. Seller assumes no obligation or liability for the information in this document. NO WARRANTIES ARE GIVEN; ALL IMPLIED WARRANTIES OF MERCHANTABILITY OR FITNESS FOR A PARTICULAR PURPOSE ARE EXPRESSLY EXCLUDED.