Density (23°C)
|
1.05
|
g/cm³
|
ISO 1183/A |
Melt Mass-Flow Rate (MFR) (230°C/5.0 kg)
|
9.0
|
g/10 min
|
ISO 1133 |
Melt Volume-Flow Rate (MVR) (230°C/5.0 kg)
|
10
|
cm³/10min
|
ISO 1133 |
Tensile Modulus (23°C)
|
2800
|
MPa
|
ISO 527-1 |
Tensile Stress (Yield, 23°C)
|
36.0
|
MPa
|
ISO 527-2 |
Tensile Strain (Yield, 23°C)
|
5.0
|
%
|
ISO 527-2 |
Flexural Modulus 2 (23°C)
|
2900
|
MPa
|
ISO 178/A |
Charpy Notched Impact Strength (23°C)
|
4.5
|
kJ/m²
|
ISO 179/1eA |
Charpy Unnotched Impact Strength (23°C)
|
50
|
kJ/m²
|
ISO 179/1eU |
Deflection Temperature Under Load (0.45 MPa, Unannealed)
|
115
|
°C
|
ISO 75-2/B |
Deflection Temperature Under Load (1.8 MPa, Unannealed)
|
65.0
|
°C
|
ISO 75-2/A |