Density
|
1.23
|
g/cm³
|
ISO 1183 |
Melt Volume-Flow Rate (MVR) (360°C/10.0 kg)
|
30
|
cm³/10min
|
ISO 1133 |
Molding Shrinkage
|
|
|
ISO 294-4 |
Across Flow
|
0.77
|
%
|
|
Flow
|
0.72
|
%
|
|
Water Absorption (Saturation, 23°C)
|
0.80
|
%
|
ISO 62 |
Water Absorption (Equilibrium, 23°C, 50% RH)
|
0.30
|
%
|
ISO 62 |
Tensile Modulus (23°C)
|
2550
|
MPa
|
ISO 527-1 |
Tensile Stress (Yield, 23°C)
|
75.0
|
MPa
|
ISO 527-2 |
Tensile Strain (Yield, 23°C)
|
5.7
|
%
|
ISO 527-2 |
Charpy Notched Impact Strength
|
|
|
ISO 179 |
-30°C
|
6.5
|
kJ/m²
|
|
23°C
|
6.0
|
kJ/m²
|
|
Charpy Unnotched Impact Strength
|
|
|
ISO 179 |
-30°C
|
No Break
|
|
|
23°C
|
No Break
|
|
|
Notched Izod Impact Strength
|
|
|
ISO 180 |
-30°C
|
6.5
|
kJ/m²
|
|
23°C
|
6.0
|
kJ/m²
|
|
Ball Indentation Hardness
|
135
|
MPa
|
ISO 2039-1 |
Deflection Temperature Under Load (1.8 MPa, Unannealed)
|
177
|
°C
|
ISO 75-2/A |
CLTE -
Flow
|
5.3E-5
|
cm/cm/°C
|
|
Surface Resistivity
|
> 1.0E+15
|
ohms
|
IEC 60093 |
Volume Resistivity
|
> 1.0E+15
|
ohms·cm
|
IEC 60093 |
Electric Strength
|
37
|
kV/mm
|
IEC 60243-1 |
Dielectric Constant
|
|
|
IEC 60250 |
100 Hz
|
3.50
|
|
|
1 MHz
|
3.40
|
|
|
Dissipation Factor
|
|
|
IEC 60250 |
100 Hz
|
1.1E-3
|
|
|
1 MHz
|
7.1E-3
|
|
|
Comparative Tracking Index
|
125
|
V
|
IEC 60112 |